80% 10-220mm Ferrovanadium Description
When smelting ferrovanadium 80% in an electric furnace, iron scrap, V2O5 in the form of fused pieces (or calcium vanadate in the form of briquettes), crushed ferrosilicon (65-76% Si) and lime are introduced into the furnace to slag the resulting silicic acid. In the aluminothermic method, V2O5 (or ferrovanadate) is mixed with 30-40% (by weight) of iron oxide and aluminum powder (0.7-0.9 kg per 1 kg of ferrovanadium), lime and fluorspar (flux), placed in molds and ignited with thermite (for example, iron-aluminum, which is a mixture of Fe3O4 and Al powder), ignited using a voltaic arc.
![]()
80% 10-220mm Ferrovanadium Manufacturers
The Specification Of 80% 10-220mm Ferrovanadium
| 46,6%-34,6% | |
| 1,8% | |
| 0,4% | |
| 0,2% | |
| 0,01% | |
| 0,2% | |
| 0,07% | |
| 0,02% | |
| 48-60% | |
| 2,7% | |
| 0,2% |
![]()
80% 10-220mm Ferrovanadium Customized
![]()
80% 10-220mm Ferrovanadium Price
Etichetta sexy: 80% 10-220mm ferrovanadium, China 80% 10-220mm ferrovanadium manufacturers, suppliers